IN625 Inconel 625 Superalloy Powder for SLM | High-Temperature AM Material | Forgecise

Process Type: IN625 Inconel 625 Superalloy Powder

Specifications

Login Login to view technical data

Resources

No document available.

REQUEST A QUOTE

Product Description

CategoryParameterValue / Range
Typical ApplicationsSuitable ComponentsAero- and space engine casings, guide vanes, mounting flanges, cylinders, fuel manifolds, and other high-performance parts
Applicable ProcessesAdditive ManufacturingSLM (Selective Laser Melting), LSF (Laser Solid Forming)
Chemical Composition (wt.%)C≤ 0.1
Cr20.0–23.0
NiBalance
Co≤ 1.0
Nb3.15–4.15
Mo8.0–10.0
Al≤ 0.4
Ti≤ 0.4
Fe≤ 5.0
Si≤ 0.5
Mn≤ 0.5
S≤ 0.015
P≤ 0.015
Cu≤ 0.07
O≤ 0.02
N≤ 0.02
Physical PropertiesParticle Size (D10 / D50 / D90)≥15 μm / 30–40 μm / ≤60 μm
Sphericity≥ 0.9
Apparent Density (g/cm³)≥ 4.4
Tap Density (g/cm³)≥ 5.0
Flowability (s/50g)≤ 18
Mechanical Properties (Heat-Treated)Test TemperatureRoom Temp / 815°C
Tensile Strength (MPa)≥ 830 / ≥ 350
Yield Strength (MPa)≥ 410 / ≥ 240
Elongation (%)≥ 35.0 / ≥ 30.0

1. Advantages and Features of This IN625 (Inconel 625) Superalloy Powder

1.1 Optimized for Industrial Applications

IN625 powder is specifically engineered for demanding aerospace and space applications requiring exceptional high-temperature performance and corrosion resistance. With long-term service capability up to 815°C, this nickel-based superalloy powder is ideal for manufacturing critical components such as aero-engine casings, guide vanes, mounting flanges, cylinders, fuel manifolds, and other high-performance parts through additive manufacturing.

1.2 Excellent SLM Processability

The powder’s optimized particle size distribution (D10 ≥15 μm / D50 30–40 μm / D90 ≤60 μm) ensures superior flowability (≤18 s/50g) and excellent powder bed uniformity during SLM processing. High sphericity (≥0.9) minimizes satellite particles and promotes consistent layer spreading, resulting in defect-free printed components with minimal porosity and excellent surface finish.

1.3 Robust Mechanical Performance

IN625 delivers outstanding mechanical properties across temperature ranges. At room temperature, it achieves tensile strength ≥830 MPa, yield strength ≥410 MPa, and elongation ≥35.0%. Even at elevated temperatures of 815°C, it maintains impressive performance with tensile strength ≥350 MPa, yield strength ≥240 MPa, and elongation ≥30.0%, ensuring structural integrity in extreme environments.

1.4 Stable Physical Properties

Consistent powder characteristics including apparent density ≥4.4 g/cm³ and tap density ≥5.0 g/cm³ guarantee reliable packing behavior and predictable thermal conductivity during the SLM process. These stable physical properties contribute to uniform heat distribution and controlled solidification, minimizing residual stress and distortion.

1.5 High Purity & Compositional Control

Strict control of interstitial elements (O ≤0.02%, N ≤0.02%, S ≤0.015%, P ≤0.015%) ensures optimal high-temperature strength and corrosion resistance. The balanced composition with precise chromium (20.0–23.0%), molybdenum (8.0–10.0%), and niobium (3.15–4.15%) content provides excellent oxidation resistance while maintaining weldability and fabricability.

2. IN625 (Inconel 625) Superalloy Powder Material Overview

2.1 Chemical Composition Characteristics

IN625 is a nickel-based solid solution strengthened superalloy with the following composition (wt.%):

  • Nickel (Ni): Balance (primary matrix element)
  • Chromium (Cr): 20.0–23.0% (provides oxidation and corrosion resistance)
  • Molybdenum (Mo): 8.0–10.0% (enhances strength and creep resistance)
  • Niobium (Nb): 3.15–4.15% (provides precipitation strengthening)
  • Iron (Fe): ≤5.0% (cost-effective strengthening element)
  • Cobalt (Co): ≤1.0% (improves high-temperature stability)
  • Carbon (C): ≤0.1% (grain boundary strengthening)
  • Trace Elements: Ti ≤0.4%, Al ≤0.4%, Si ≤0.5%, Mn ≤0.5%, Cu ≤0.07%
  • Interstitials: O ≤0.02%, N ≤0.02% (strictly controlled for optimal properties)

2.2 Powder Characteristics

  • Particle Size Distribution: D10 ≥15 μm, D50 30–40 μm, D90 ≤60 μm
  • Morphology: High sphericity ≥0.9 with smooth surfaces
  • Density: Apparent density ≥4.4 g/cm³, Tap density ≥5.0 g/cm³
  • Flowability: ≤18 seconds per 50 grams (Hall flowmeter)
  • Oxygen Content: ≤0.02% (maintains ductility and weldability)

3. Technical Advantages

IN625 powder offers several key technical advantages for SLM applications:

  • Superior High-Temperature Strength: Maintains mechanical integrity up to 815°C, making it ideal for hot-section components
  • Excellent Corrosion Resistance: Chromium and molybdenum content provide exceptional resistance to pitting, crevice corrosion, and stress corrosion cracking
  • Outstanding Fabricability: Good weldability and formability enable complex geometries and post-processing operations
  • Controlled Thermal Expansion: Balanced composition ensures predictable thermal behavior during heating and cooling cycles
  • Consistent Print Quality: Optimized powder characteristics minimize defects and ensure repeatable manufacturing results
  • Versatile Process Compatibility: Suitable for both SLM and LSF (Laser Solid Forming) processes

4. SLM Process Parameter Recommendations

For optimal results when processing IN625 powder via SLM:

  • Laser Power: 280–450 W (depending on layer thickness and feature size)
  • Scan Speed: 800–1300 mm/s
  • Hatch Spacing: 80–120 μm
  • Layer Thickness: 30–50 μm
  • Scan Strategy: Island scanning or chessboard pattern to minimize residual stress
  • Preheat Temperature: 80–150°C (reduces thermal gradients and distortion)
  • Atmosphere: Argon or nitrogen with oxygen content <100 ppm
  • Build Orientation: Consider thermal management and support structure requirements for overhangs
  • Energy Density: 40–60 J/mm³ (adjust based on specific equipment and part geometry)

5. Post-Processing Procedures

Recommended post-processing steps for IN625 SLM components:

  1. Stress Relief Annealing: 1095–1120°C for 1–2 hours, followed by rapid cooling (water quench or air cool)
  2. Solution Annealing (if required): 1150°C for 1 hour, rapid cooling per AMS 5666/ASTM B446 standards
  3. Support Removal: Mechanical or EDM methods for delicate features
  4. Surface Finishing: Grinding, polishing, or shot peening as needed
  5. Quality Inspection: Dimensional verification, surface roughness measurement, and non-destructive testing
  6. Final Heat Treatment: Depending on specific application requirements

6. Performance Specifications

Mechanical Properties (Heat-Treated Condition)

PropertyRoom Temperature815°C
Tensile Strength≥830 MPa≥350 MPa
Yield Strength (0.2%)≥410 MPa≥240 MPa
Elongation≥35.0%≥30.0%

Physical Properties

  • Density: ~8.44 g/cm³ (bulk material)
  • Melting Range: 1290–1350°C
  • Thermal Conductivity: ~9.8 W/m·K at 100°C
  • Coefficient of Thermal Expansion: ~12.9 × 10⁻⁶/°C (20–100°C)

7. Application Areas

IN625 powder is particularly suited for:

  • Aerospace: Engine casings, guide vanes, mounting flanges, fuel manifolds, turbine components
  • Space: Rocket engine components, satellite propulsion systems, thermal protection systems
  • Energy: Gas turbine components, heat exchangers, nuclear reactor parts
  • Industrial: Chemical processing equipment, marine components, oil and gas applications
  • Research & Development: Prototype testing, material validation, process optimization studies

8. Comparison with Similar Powders

ParameterIN625Hastelloy XInconel 718Haynes 230
Max Service Temp815°C900°C700°C1150°C
Tensile Strength (RT)≥830 MPa≥700 MPa≥1200 MPa≥800 MPa
Corrosion ResistanceExcellentGoodGoodExcellent
FabricabilityExcellentExcellentGoodModerate
CostModerateModerateHighVery High
SLM SuitabilityExcellentExcellentGoodGood
Nb Content3.15–4.15%None5.0–5.5%None

9. Precautions

When working with IN625 powder for SLM:

  • Powder Handling: Use appropriate PPE and follow safety protocols for metal powder handling
  • Storage: Store in sealed containers under inert atmosphere to prevent moisture absorption and oxidation
  • Recycling: Limit powder reuse cycles to maintain consistent properties; monitor oxygen content regularly
  • Thermal Management: Account for high thermal conductivity during build planning to avoid overheating
  • Support Structures: Design adequate supports for overhangs and thin features to prevent warpage
  • Post-Processing: Plan for potential distortion during stress relief and heat treatment operations
  • Heat Treatment: Follow AMS 5666/ASTM B446 standards for optimal mechanical properties

10. Summary

IN625 powder, also known as Inconel 625 powder, is a premium nickel-based superalloy specifically engineered as additive manufacturing powder for selective laser melting (SLM) applications. This high-temperature alloy powder offers exceptional corrosion resistance and high-temperature strength, making it ideal for aerospace AM materials and critical aero-engine components such as gas turbine powder applications. As a nickel-chromium-molybdenum powder with spherical superalloy powder morphology, it ensures optimal SLM processability and consistent build quality. The heat-resistant powder is perfect for demanding metal AM powder requirements in chemical processing powder applications, and Forgecise customization services can tailor AM material specifications to meet specific project needs, whether for research, prototyping, or industrial-scale production of high-performance components requiring oxidation resistant powder characteristics.
IN625 (Inconel 625) superalloy powder represents an excellent choice for SLM manufacturing of high-performance components requiring exceptional corrosion resistance, good high-temperature strength up to 815°C, and reliable mechanical performance. Its optimized powder characteristics ensure excellent processability, while the balanced chemical composition with niobium strengthening provides the ideal combination of strength, corrosion resistance, and thermal stability for demanding aerospace, space, and industrial applications. With proper process parameters and post-processing, IN625 enables the production of complex, high-performance components that would be difficult or impossible to manufacture using traditional methods.

11. Customization Services by Forgecise

Forgecise delivers comprehensive superalloy powder customization solutions, spanning the complete spectrum from standard high-temperature formulations to customer-specific high-performance nickel-based superalloys. We support mainstream superalloy grades including Haynes 230, Inconel series, and Hastelloy variants, with the capability to precisely tailor chemical composition, particle size distribution, sphericity, oxygen/nitrogen content, and thermal expansion coefficient to match your exact industrial and manufacturing requirements. Our superalloy powders are optimized for demanding additive manufacturing processes including SLM and EBM, ensuring consistent printability, high density, superior high-temperature mechanical properties, and reliable performance in your final aerospace, energy, and industrial components.

FAQ:

Key Features

High Speed, High Precision, High Quality

Laboratory setting showing gloved hands holding innovative 3D printed metal structures.
Forgecise Metal 3D Printers – SLM Series
Excellent as-built surface finish – Parts achieve good surface quality without post-polishing.
High dimensional accuracy – Ideal for producing precision prototypes.
Direct fabrication of metal end-use parts – Eliminates intermediate steps.
Fully dense metallurgical structure (>99% density) – Eliminating the need for post-processing.
Rapid build times – Parts can be completed depending on size and complexity.
Complex geometries made possible – Functional features such as snap-fits and living hinges can be printed directly.
Broad material compatibility – Supports a wide range of metal powders.
Perfect for custom, low-volume production – small-batch manufacturing.

Get a Customized Quote

This field is required.
This field is required.
This field is required.